WCT-20CrC6Ni Thermal Spray Powder
WCT 74/20/6 Series
Tungsten carbide, chrome carbide
and nickel thermal spray powders manufactured by BTI are an agglomerated
and sintered material, which provide superior oxidation, corrosion and
chemical resistance.
This powder can withstand temperatures up to
750 C.
The base tungsten carbide (WC) powder used to produce this material is
typically a 2-5 microns APS conventional carbide powder, but micrograin (0.2-0.3
microns APS) carbide powder can also be used in whole or in part.
|
WCT-20CrC6Ni (conventional WC)
WCTN-20CrC6Ni (micrograin WC)
|
|
DESCRIPTION
|
Agglomerated & Sintered
|
|
CHEMICAL
|
Cr = 16.0 – 18.0%
Ni = 5.0 – 7.0%
C = 6.5 – 7.5%
W = Balance
|
|
AVAILABLE SIZES
|
-53 +20 micron
-45 +15 micron
-30+5 micron
|
|
APPARENT DENSITY
|
3.5
g/cc minimum
|
Analytical ReportsA Certificate of Analysis (COA) accompanies each shipment. |